Alloy Digest (2019) 68 (4): TS-763.
Published: 01 April 2019
... Sandvik APM 2730 is a powder metallurgical alloyed hot-isostatic-pressed high-speed tool steel with abrasive wear resistance and high-compressive strength. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and...
Journal Articles
Alloy Digest (2009) 58 (7): SS-1038.
Published: 01 July 2009
... Kanthal APM HP is an advanced high-purity powder metallurgical dispersion-strengthened resistance heating or high-temperature alloy of the family FeCrAlMo that has good form stability at high temperatures. This datasheet provides information on composition, physical properties, hardness...