Skip Nav Destination
Close Modal
Search Results for
Sandvik 8R70
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for Sandvik 8R70
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1997) 46 (5): SS-683.
Published: 01 May 1997
... Sandvik 8R70 is a molybdenum-containing austenitic stainless steel that is stabilized with an addition of titanium to prevent intergranular attack. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Abstract
View articletitled, <span class="search-highlight">SANDVIK</span> <span class="search-highlight">8R70</span>: Titanium-Stabilized Austenitic Stainless Steel
View
PDF
for article titled, <span class="search-highlight">SANDVIK</span> <span class="search-highlight">8R70</span>: Titanium-Stabilized Austenitic Stainless Steel
Sandvik 8R70 is a molybdenum-containing austenitic stainless steel that is stabilized with an addition of titanium to prevent intergranular attack. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-683. Producer or source: Sandvik.