1-4 of 4 Search Results for

Sandvik 3R12

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (9): SS-612.
Published: 01 September 1995
... Sandvik 3R12 is an austenitic chromium-nickel stainless steel with extra low carbon content. It is superior to Type 302 in corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (7): SA-482.
Published: 01 July 1996
... Sandvik 3R12/4L7 is a composite tube consisting of type 304L stainless steel for corrosion resistance on the outside diameter and having carbon steel (A210 Gr. A1) as the inside component for both water wetted service and the design load. The major application is tubing to handle the corrosive...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1995) 44 (10): SS-614.
Published: 01 October 1995
... that it is necessary to read the cutting data to make full use of SANMAC 316L. Recommended insert grades from Sandvik Coromant can be seen from Figures 1 and 2. Corrosion Resistance: General corrosion Sandvik 3R12 has good resistance in: organic acids at high concentrations and moderate temperatures; inorganic acids...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (11): SS-491.
Published: 01 November 1987
... be utilized. DOI: 10.31399/asm.ad.ss0491 Copyright ┬ę ASM International┬« 1996 Temperature. C ( FI CPT C, (OF) 400 mV SCE I Boiling potnt CUrVe -0 -=I- Sandvlk 2RElg 413ot (105) 0 20 40 60 80 100 % HNOJ Fig. 1 - Isocorrosion in nitric acid (O.lmm/yr) (Impy) SANDVIK 2RElO and 3R12 (AISI Type 304L). Corrosion...