Alloy Digest (2006) 55 (7): CS-146.
Published: 01 July 2006
... Sandvik 20C is a strip steel with high fatigue strength, supplied for pad printing or as a shock absorber steel. It has a high yield to tensile strength value. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also...