Alloy Digest (2020) 69 (3): SS-1316.
Published: 01 March 2020
... Sandmeyer Alloy 410 (UNS S41000) is a general purpose 12% chromium martensitic stainless steel that can be heat treated to obtain a wide range of mechanical properties. This alloy possesses good corrosion resistance along with high strength and hardness. This datasheet provides information...
Journal Articles
Alloy Digest (2020) 69 (7): SS-1322.
Published: 01 July 2020
... Sandmeyer 410S (UNS S41008) is a 13% chromium, ferritic stainless steel. It is a low carbon, non-hardening modification of Type 410 stainless steel. This non-hardening characteristic helps prevent cracking when the alloy is exposed to high temperatures or welded. This datasheet provides...
Journal Articles
Alloy Digest (2020) 69 (11): SS-1329.
Published: 01 November 2020
... Copyright © ASM International® 2020 2020 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat treatability high temperature alloys joinability low-temperature alloys machinability Outokumpu Moda 410S/4000 physical properties tensile properties...