Skip Nav Destination
Close Modal
Search Results for
SWISSMETAL SM118N
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-17 of 17 Search Results for
SWISSMETAL SM118N
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2002) 51 (4): Cu-679.
Published: 01 April 2002
... Swissmetal SM117N (58T), SM118N (58A), SM121N (58F) alloys are free-machining brasses with increasing copper content for increasing cold formability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Abstract
View article
PDF
Swissmetal SM117N (58T), SM118N (58A), SM121N (58F) alloys are free-machining brasses with increasing copper content for increasing cold formability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: CU-679. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2001) 50 (6): Cu-668.
Published: 01 June 2001
...: Modulus of elasticity, GPa (106 psi) 11.5 (16.7) See also Table 1. Heat Treatment: Anneal at 500 °C (932 °F) for 1 h at temperature. Stress relieve at 200 °C (390 °F) for 4 h at temperature. Fabricability: Cold working Good Capacity for hot working Moderate Machining rating compared to SM118N Good, 60...
Abstract
View article
PDF
Swissmetal SM453C is a free-machining copper alloy with high electrical conductivity. It is recommended for male contacts in electrical and electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-668. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2002) 51 (3): Cu-677.
Published: 01 March 2002
.... Heat Treatment: Anneal at 500 °C (932 °F) for 1 h at temperature. Stress relieve at 250 °C (482 °F) for 4 h at temperature. Fabricability: Cold working Middle Capacity for hot working Good Machining rating compared to Good, 85 SM118N free-machining brass (CuZn39Pb3) = 100 Tool life compared to free...
Abstract
View article
PDF
Swissmetal alloy SM163N is a free-machining brass with good formability. Typical applications include any part made by a combination of machining and a light cold deformation such as thread rolling, bending, and/or riveting. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-677. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2001) 50 (3): Cu-661.
Published: 01 March 2001
... compared to SM118N free-machining brass (CuZn39Pb3) = 100 Moderate; 75 Tool life compared to free machining brass = 110 Good; 80 Tendency to form short chips compared to free-cutting brass = 90 Moderate; 70 Suitability for polishing Good Suitability for plating Good Weldability: Capacity for soft soldering...
Abstract
View article
PDF
Swissmetal alloy SM195N is a free-machining brass with higher conductivity than more common free-machining brasses. It is used for electronic contacts. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-661. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2000) 49 (10): Cu-654.
Published: 01 October 2000
... Capacity for hot working Good Machining, compared with SM118N Good; 90 free-machining brass (CuZn39Pb3) as 100, % Tool life, compared with free machining Good; 90 brass as 100, % Tendency for shirt chips, compared with Good; 90 free-cutting brass as 90, % Suitability for polishing Good Suitability...
Abstract
View article
PDF
Swissmetal alloy SM206J is a free-machining nickel silver that can be readily cold formed. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming. Filing Code: CU-654. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2000) 49 (12): Cu-646.
Published: 01 December 2000
... for hot working Middle Machining rating compared to SM118N free-machining brass (CuZn 39Pb3, C385) = 100 Very good , 90 Tool life compared to free-machining brass = 100 Good, 80 Tendency to form short chips com- pared to free cutting brass = 90) Very good, 90 Suitability for polishing Excellent...
Abstract
View article
PDF
Swissmetal alloy SM900R is a free-machining nickel-free copper alloy with high yield strength and high mechanical strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-646. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2001) 50 (4): Cu-663.
Published: 01 April 2001
... (1295 °F) for 5 min at temperature. Fabricability: Cold working Good Capacity for hot working Moderate to weak Machining rating compared to SM118N free machining brass (CuZn39Pb3) = 100 Moderate, 70 Tool life compared to free machining brass = 110 Moderate, 70 Tendency to form short chips compared...
Abstract
View article
PDF
Swissmetal alloy SM451C is a free machining, heat treatable leaded nickel-copper alloy with mechanical strength and electrical conductivity. It is used in spring contacts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming and joining. Filing Code: CU-663. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2001) 50 (5): Cu-665.
Published: 01 May 2001
... of elasticity, guaranteed for 118 (17) rods, GPa (106 psi) See also Table 1. Heat Treatment: Anneal at 550 °C (1020 °F) for 1 h at temperature. Stress relieve at 240 °C (465 °F) for 4 h at temperature. Fabricability: Cold working Good Capacity for hot working Bad Machining rating compared to SM118N Very good...
Abstract
View article
PDF
Swissmetal alloy SM800K is a free-machining phosphor bronze with high mechanical strength and excellent free-machining quality. It is recommended for the manufacture of spring contacts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-665. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2001) 50 (1): Cu-657.
Published: 01 January 2001
.... Fabricability: Cold working Good Capacity for hot working Good Machining rating compared to SM118N Good, 80 free-machining brass (CuZn39Pb3) = 100 Tool life compared to free-machining Good, 80 brass = 110 Tendency to form short chips compared to Good, 90 free-cutting brass = 90 Suitability for polishing Good...
Abstract
View article
PDF
Swissmetal SM184N is a free-machining brass alloy with an optimal combination of machinability and cold deformability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-657. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2002) 51 (7): Cu-685.
Published: 01 July 2002
... cold work when solution annealed Capacity for hot working Excellent, use temperature range 800 850 °C (1472 1562 °F) Machining rating compared to Fair, 30 precipitation SM118N free cutting brass hardened (CuZn39Pb3) = 100 Tool life compared to free- Good, 80 machining brass = 110 Weldability: Capacity...
Abstract
View article
PDF
Swissmetal alloy SM468C is a heat treatable copper alloy with high strength and hardness. It has good corrosion resistance and relatively good conductivity. It is used in electrical generators. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: CU-685. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2002) 51 (12): Cu-695.
Published: 01 December 2002
... relieve at 250 350 °C (480 660 °F). Fabricability: The hot working range is 670 730 °C (1240 1345 °F) with the optimum at 680 700 °C (1250 1290 °F). Capacity for cold working Low (less suitable, 15% max cold reduction) Capacity for hot working Excellent Machining rating compared to Good, 70 SM118N free...
Abstract
View article
PDF
Swissmetal alloy SM931R is an alloy designed for hot working and contains a duplex alpha plus beta microstructure. The alloy has also been called DORECO. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength. It also includes information on forming, heat treating, and joining. Filing Code: CU-695. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2002) 51 (6): Cu-683.
Published: 01 June 2002
...) for 4 h at temperature. Fabricability: Capacity for cold working Good Capacity for hot working Good Machining rating compared to Middle to good, 80 SM118N free-cutting brass (CuZn39Pb3) = 100 Tool life compared to Middle to good, 80 free-machining brass = 110 Tendency to form short chips Good, 75...
Abstract
View article
PDF
Swissmetal alloy SM158N (Boillat 61B) is a free-machining brass with both machinability and cold workability. The alloy has been called heavy-leaded brass, clock brass, and engraver’s brass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-683. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2002) 51 (11): Cu-693.
Published: 01 November 2002
... at temperature. Stress relieve at 250 °C (480 °F) for 4 h at temperature. Fabricability: Capacity for cold working Very good Capacity for hot working Middle to good Machining rating compared to SM118N free-cutting brass (CuZn39Pb3, C360) = 100 SM185N 70 SM188N 65 Tool life compared to free-machining brass = 110...
Abstract
View article
PDF
The Swissmetal alloys SM185N (62B) and SM188N (62C) are free-machining brasses with good cold-forming capabilities. The alloys have been called medium- and low-leaded brass, respectively. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-693. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2001) 50 (2): Cu-658.
Published: 01 February 2001
.... Stress relieve at 250 °C (480 °F) for 4 h at temperature. Fabricability: Cold working Moderate Capacity for hot working Good Machining rating compared to SM118N Excellent, 100 free-machining brass (CuZn39Pb3) = 100 Tool life compared to free-machining Excellent, 110 brass = 110 Tendency to form short...
Abstract
View article
PDF
Swissmetal alloys SM154N, 150N and 184N are brass alloys with high copper content and good cold forming. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-658. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2002) 51 (9): Cu-688.
Published: 01 September 2002
... 840 (1400 1545) °C (°F) Machining rating compared to Fair, 30 as age hardened SM118N free-cutting brass (CuZn39Pb3, C360) = 100 Weldability: Capacity for soldering Good Brazing Good Oxyacetylene welding Good Gas-shielded arc welding Good Capacity for resistance butt welding Good Capacity...
Abstract
View article
PDF
Swissmetal alloy SM466C is a Cu-Ni-Si alloy that is age hardenable to medium strength while maintaining a relatively high electrical conductivity. The alloy is readily hot stamped and used in railroad bolting. The alloy is also called Nibrofor I and Sikudor I. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: CU-688. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2000) 49 (7): Cu-651.
Published: 01 July 2000
...% max cold reduction. Hot working is also excellent with a hot working temperature range of 750 850 °C (1382 1562 °F). Machining is very poor at 30% that of SM118N (CuZn39Pb3) or Condition D. Suitability for polish- ing is good, and suitability for plating is excellent. The annealing temperature range...
Abstract
View article
PDF
Swissmetal alloy CuNi1P is age-hardenable for strength but retains good electrical/thermal properties with good formability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: CU-651. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.
Journal Articles
Alloy Digest (2002) 51 (8): Cu-687.
Published: 01 August 2002
... Fabricability: Capacity for cold working, cold Excellent, 90% reduction max Capacity for hot working Very poor Machining rating compared to Moderate SM118N free-cutting brass (CuZn39Pb3) = 100 Suitability for polishing Good Suitability for plating Excellent Weldability: Capacity for soldering Excellent Brazing...
Abstract
View article
PDF
Swissmetal alloy SM275H is a hardenable Cu-Ni-Sn alloy with good workability and corrosion resistance. It is often used in the automotive industry for springs, contacts, and clips. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CU-687. Producer or source: Swissmetal Metalworks Ltd, Plant Boillat.