Alloy Digest (1977) 26 (8): TS-322.
Published: 01 August 1977
... SUPER MOTUNG 33 is one of the heavy-duty high-speed steels. It is recommended for machining materials of high hardness. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and surface treatment...
Journal Articles
Alloy Digest (1960) 9 (2): TS-9.
Published: 01 February 1960
... SUPER-MOTUNG, a molybdenum type of high-speed steel containing cobalt, possesses a combination of cutting and toughness properties superior to many grades of high-speed steels. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes...