Alloy Digest (1989) 38 (5): P-3.
Published: 01 May 1989
... SUPEC G401 AND G402 are resins based on polyphenylene sulfide (PPS) technology. They combine long-and short-term heat resistance with broad chemical resistance and they are inherently flame retardant. This datasheet provides information on physical properties, hardness, elasticity, and tensile...