Alloy Digest (2015) 64 (7): CS-191.
Published: 01 July 2015
... Sumitomo SM125S is a low alloy high strength carbon steel for use in oil country tubular goods as a material suitable for medium severity sour service. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2015) 64 (6): CS-190.
Published: 01 June 2015
... Sumitomo SM125ES is a low alloy, high strength carbon steel for use in oil country tubular goods as a material suitable for high severity sour service. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties. It also includes information...