Alloy Digest (2017) 66 (2): SS-1257.
Published: 01 February 2017
...: Nippon Steel & Sumikin Stainless Steel Corporation Copyright ┬ę ASM International┬« 2017 2017 ASM International chemical composition formability heat treatability SUMITOMO NSSC 27A/NSSC 27AS workability NSSC 27A/NSSC 27AS are proprietary high formability austenitic stainless steels...