Alloy Digest (1994) 43 (9): SS-573.
Published: 01 September 1994
... SUMITOMO DP3W tensile properties thermal properties UNS S39274 S32740 SUMlT()MO Dp3W i%kte~ ss-573 SEPTEMBER 1994 - DIGEST A DATA ON WORLD WIDE METALS AND ALLOYS SUMITOMO DP3W pt#ahudby: Abyl3igea, lnc.1201a7.9161 ~?7CardiiStmet. m N.J. 0705OiU.SA (Austeniticlferritic duplex stainless steel) DP3W is...
Journal Articles
Alloy Digest (1999) 48 (7): SS-752.
Published: 01 July 1999
... required. The maximum heat input recommended is 2.0 kJ/mm (48 Btu/in and the maximum interpass temperature is 150 °C (300 °F). The products recom- mended for each welding method are shown in the following ta- ble. Welding method Recommended Sumitomo product Gas tungsten arc (GTAW) DP3W-T Gas metal arc...