Published: 01 April 1992
... STYRON 666D,685,685D and 697 are general purpose thermoplastic polystyrene resins produced by joining styrene monomer molecules into long polymer chains ranging from 100 to 20,000 monomer units per chain. They are noncrystalline. This datasheet provides information on composition, physical...