Alloy Digest (1972) 21 (10): SA-281.
Published: 01 October 1972
... STROLOY 503-A is a through-hardening steel developed for bearing races. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-281. Producer or source...
Journal Articles
Alloy Digest (1985) 34 (2): SA-406.
Published: 01 February 1985
... STROLOY 503-A is a hypereutectoid steel of bearing quality. It has through-hardening characteristics similar to those of AISI 52100 steel. Stroloy 503-A is made in accordance with ASTM A 295-84. It is used principally in ball bearing applications. This datasheet provides information on composition...