Alloy Digest (2016) 65 (12): SA-773.
Published: 01 December 2016
... Strenx 1100 MC is a high-strength hot-rolled structural steel made for cold forming, with minimum yield strength of 1100 MPa (160 ksi) for stronger and lighter structures. This alloy meets or exceeds the requirements of S1100 MC in EN 10149-2. This datasheet provides information on composition...