Alloy Digest (1993) 42 (6): Co-92.
Published: 01 June 1993
... STELLITE 31 PM is a cobalt-base alloy with 7.5 wt% W recommended for handling severe conditions of abrasion, heat and corrosion. The PM designation indicates prealloyed atomized powders and parts made from the powder. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1993) 42 (8): Co-93.
Published: 01 August 1993
... STELLITE STAR J-METAL PM (UNS R30102) is a cobalt-base alloy recommended for handling severe conditions of abrasion, heat and corrosion. The PM designation indicates prealloyed atomized powders and parts made from the powder. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1993) 42 (3): Co-90.
Published: 01 March 1993
... STELLITE 3 PM (UNS R30103) is a cobalt-base alloy recommended for handling severe conditions of abrasion, heat and corrosion. The PM designation indicates prealloyed atomized powders and parts made from the powder. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2019) 68 (12): Co-87.
Published: 01 December 2019
.... The PM designation indicates pmalloyed atomized powders and parts made from the powder. STELLITE@ is a registered trademark. Composltion, Nominal Wt., %: Nickel 3 max. Silicon 1 max. Iron 3max. Manganese 1 max. Chromium 31 Tungsten 10.5 Carbon 1.9 Boron 1.0 max. Other 2.0max. Cobalt Bal. Physical...
Journal Articles
Alloy Digest (1993) 42 (7): Ni-435.
Published: 01 July 1993
... and wear resistance as well as machining and joining. Filing Code: Ni-435. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition DELORO 716 PM hardness high-temperature alloys...
Journal Articles
Alloy Digest (1993) 42 (2): Ni-422.
Published: 01 February 1993
... resistance as well as machining and joining. Filing Code: Ni-422. Producer or source: Deloro Stellite Inc. Producer or Source: Deloro Stellite Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition DELORO N-6 PM hardness joinability machinability physical...
Journal Articles
Alloy Digest (1961) 10 (8): Co-29.
Published: 01 August 1961
... for finishing. Wiisor KS caolsnt (IS puts aster co 1 psrc oil) is recommended for cumisg, while a coolsst of 1 put soluble oil co 1 psrt kerosene is recoatmen ded for drilling. Wheel I Removing stock Norton Sharp comer work Pm&ion Straight mdius work Coolant 1 gal. soluble oil + 50 gal. water + l/z lb...
Journal Articles
Alloy Digest (1982) 31 (3): Ni-274.
Published: 01 March 1982
... carbide to& 10-2.5 SFPM (0.050.13 m/s) baud on number of threads per inch (mm). low C-3 tungsten carbide to& Coolant-water base tlti diluted 15 pars water to one pm fluid. TOOIS for fa& and hdng are basically the same s turning tools except for greatn clearances where needed 2C-2 tungsten carbide twist...
Journal Articles
Alloy Digest (1971) 20 (9): Ti-63.
Published: 01 September 1971
... in a single operation. Powdered graphite is used as the draw lubricant at this temperature. Multistage drawing can be accomplished at room temperature with intermediate anneals at 1OOoOF. Waldability: A-70 can be welded by common methods but certain pm- cautions are necessary. AU fusion welding requires...