Alloy Digest (2011) 60 (2): Co-121.
Published: 01 February 2011
... physical properties powder metal products STELCAR JET KOTE 117 wear resistance DATA ON WORLDWIDE METALS AND ALLOYS Copyright ┬ę 2011, ASM International┬«. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH...