Alloy Digest (1961) 10 (12): TS-112.
Published: 01 December 1961
... STAR-M0 M-2 is a tungsten-molybdenum high-speed steel of the 6-6-2 type having good red-hardness quality. This alloy corresponds to AISI type M2. Star-M0 is also available in Free-Machining type, to which sulfur, in the form of alloy sulphides, has been added for better machinability and increased...