Journal Articles
Alloy Digest (2021) 70 (10): SA-876.
Published: 01 October 2021
... SSAB Ramor 400 is a low-carbon, chromium-molybdenum-nickel-boron alloy protection steel that is used in the heat treated condition (Hardness = 360–460 HBW) for blast protection. This datasheet provides information on composition, hardness, tensile properties, and bend strength. It also includes...