1-20 of 20 Search Results for

SPRAYWELD Process

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1974) 23 (6): Ni-205.
Published: 01 June 1974
... COLMONOY No. 62SA comprises a nickel-base alloy recommended for hard surfacing parts to resist wear, corrosion, heat and galling. Colmonoy No. 62SA is supplied as atomized powder for application with Wall Colmonoy's SPRAYWELD Process. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1974) 23 (7): Ni-206.
Published: 01 July 1974
... eliminated. It is supplied as an atomized powder of application with Wall Colmonoy's SPRAYWELD Process. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on...
Journal Articles
Alloy Digest (1995) 44 (11): Ni-489.
Published: 01 November 1995
... is supplied as an atomized powder for application with Wall Colmonoy’s SPRAYWELD Process and finished by grinding. This datasheet provides information on composition, physical properties, microstructure, and hardness. It also includes information on heat treating, machining, and powder metal forms...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-495.
Published: 01 January 1996
... aplication with Wall Colmonoy’s SPRAYWELD Process. This datasheet provides information on composition, physical properties, microstructure, and hardness. It also includes information on heat treating, machining, and powder metal forms. Filing Code: Ni-495. Producer or source: Wall Colmonoy Corporation...
Journal Articles
Alloy Digest (1975) 24 (5): Ni-217.
Published: 01 May 1975
... workability, ductility and impact strength. Colmonoy No. 5 is supplied as crushed powder for application with Wall Colmonoy's SPRAYWELD Process. Also, it is supplied as bare or coated rod for either oxyacetylene or DC electric-arc (reverse polarity) application, as well as castings. This datasheet provides...
Journal Articles
Alloy Digest (1975) 24 (6): Ni-218.
Published: 01 June 1975
.... Colmonoy No. 52SA is supplied as an atomized powder for application with Wall Colmonoy's SPRAYWELD Process. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1975) 24 (12): Ni-222.
Published: 01 December 1975
... workability, ductility and impact strength. This alloy is supplied as crushed powder for application with Wall Colmonoy's SPRAYWELD Process. Also, it is supplied as castings and as bare or coated rod for either oxyacetylene of DC electic-arc (reverse polarity) application. This datasheet provides information...
Journal Articles
Alloy Digest (1976) 25 (5): Ni-227.
Published: 01 May 1976
.... Colmonoy No. 42SA is supplied as an atomized powder for application with Wall Colmonoy's SPRAYWELD Process. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on high temperature...
Journal Articles
Alloy Digest (1976) 25 (7): Ni-230.
Published: 01 July 1976
.... It is supplied as atomized powder for application with Wall Colmonoy's SPRAYWELD and FUSEWELD processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1976) 25 (10): Co-74.
Published: 01 October 1976
... SPRAYWELD and FUSEWELD processes. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1977) 26 (6): Ni-245.
Published: 01 June 1977
... workability, ductility, and impact strength. Colmonoy No. 56 is supplied as crushed powder for application with Wall Colmonoy's SPRAYWELD and FUSEWELD Processes, or by conventional plasma-spray transferred-arc. Also, it is supplied as bare rod for either oxyacetylene or TIG (Heliarc) applications. This...
Journal Articles
Alloy Digest (1996) 45 (2): Ni-500.
Published: 01 February 1996
... Rockwell C Scale: 58-63 Specific Gravity: 9.50 Melting point (matrix) 1900°F ( 1040°C) Deposition and Fusing of Metal Powder: Colmonoy alloys are sprayed on the part to be hard-surfaced as in ordinary metal with an oxyacetylene torch. The sprayweld process thus combines the controlled application of metal...
Journal Articles
Alloy Digest (1974) 23 (9): Co-71.
Published: 01 September 1974
... hard-surfacing alloy with excellent resistance to a combination of abrasion and corrosion. It has good red hardness and excellent weldability. It is supplied as an atomized powder for application with Wall Colmonoy s SPRAY- WELD* Process. *WALLEX and SPRAYWELD are registered trademarks of Wall...
Journal Articles
Alloy Digest (1998) 47 (11): Ni-547.
Published: 01 November 1998
... the Sprayweld process, Colmonoy al- loy powders are sprayed on and fused to the base metal. This procedure combines the advantages of controLled application and a true metallurgical bond. The process consists of three basic steps and an inspection procedure. Surface Preparation Prepare the surface to...
Journal Articles
Alloy Digest (1998) 47 (10): Ni-546.
Published: 01 October 1998
... rotating, pass an intense oxyacety- lene torch flame briefly over the overlaid surface (safety glasses must be worn). The flame sets up a momenm ther- mal stress in the overlay. If no cracking occurs, the bond is satisfactov. Spraywelder System. In the Sprayweld process, Colmono). alloy powders are sprayed...
Journal Articles
Alloy Digest (1998) 47 (9): Ni-545.
Published: 01 September 1998
... and fusing are done with alternate passes of the torch. Spraywelder System. In the Sprayweld process. Colmonoy Finishing Methods. Finish machine with tungsten carbide alloy powders are sprayed on and fused to the base metal tools, or surface grind with silicon or alumina See Table 1. This procedure...
Journal Articles
Alloy Digest (1995) 44 (8): Co-98.
Published: 01 August 1995
...: In the Sprayweld Process. powdered Colmonoy alloys are sprayed on, and then fused to the base metal. This combines the advantages of controlled application and true metallurgical bonding. The process consists of three basic steps (plus an inspection procedure). Prepare the surface to be sprayed by...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-429.
Published: 01 May 1993
... International® 1996 Production of Deposits: Colmonoy is produced as deposits by spray welding, high velocity oxy-fuel systems (HVOF) or plasma trans- ferred arc (PTA) applications. In the Sprayweld process, powdered Coimonoy alloys are sprayed on and then fused to the base metal. This procedure combines the...
Journal Articles
Alloy Digest (1993) 42 (6): Ni-433.
Published: 01 June 1993
.... In the Sprayweld process, powdered Colmonoy alloys are sprayed on and then fused to the base metal. This proce- dure combines the advantages of controlled application and a true metallurgical bond. The process consists of three basic steps (plus an inspection procedure). Prepare the surface to be...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-509.
Published: 01 May 1996
... alloy containing tungsten carbide in a nickel matrix with chromium borders. Hardnesses to 58 to 63 HRC can be reached. Colmonoy. ColTung, Sprayweld. and Fusewelder are registered trademarks of Wall Colmonoy Corporation. Chemical Composition, wt (Nominal) Carbon Chromium Boron Tungsten Silicon iron...