Alloy Digest (1965) 14 (8): SA-182.
Published: 01 August 1965
... SPEED ALLOY is a deep hardening chromium, molybdenum alloy steel recommended where relatively high compressive strengths are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1991) 40 (8): TS-504.
Published: 01 August 1991
... Carpenter Micro-Melt Speed-Star FM HiC M-2 alloy is a molybdenum tungsten high-speed tool steel produced by powder metallurgy techniques. It has a more uniform structure than conventionally produced high-speed steels. It has good response to heat treatment, grinds easily, possesses improved wear...
Journal Articles
Alloy Digest (1976) 25 (6): TS-303.
Published: 01 June 1976
... compressive strength drills elasticity fracture toughness gear cutters hardness heat treatability lathe tools machinability physical properties SPEED STAR wood knives workability SPEED STAR Filing Code: TS-303 Tool Steel JUNE 1976 - DATA ON WORLD WIDE METALS AND ALLOYS Psblisbd by Engineering...
Journal Articles
Alloy Digest (1991) 40 (6): TS-344.
Published: 01 June 1991
...- DATA ON WORLD WIDE METALS AND ALLOYS JANUARY 1979 F- g 4&p--p mRwwd* -by:AbyDigaLklzol%n%1e1 sPBckwmWPd& 27CdkMSbWt~NJ.07050/U.SA CARPENTER TEN STAR@ HIGH-SPEED STEEL (High-Speed Stwl; Alsl Type MIO) CARPENTER TEN STAR is a general-purpose molybdenum-bearing high-speed steel. Its excellent wear and...
Journal Articles
Alloy Digest (1996) 45 (12): TS-548.
Published: 01 December 1996
... physical properties wear resistance workability thermal properties 1 CARPENTER I- k%Zf=k< MICRO-MELT@ HS-30 g - DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS CARPENTER MICRO-MELT@ HS-30 ALLOY (High-Alloy High-Speed Steel) Carpenter Micro-Melt I-IS-30 is an 8.5% cobalt high-ha&stability tungsten...
Journal Articles
Alloy Digest (1974) 23 (11): TS-278.
Published: 01 November 1974
... VASCO M-50 is a hardenable (martensitic), low-alloy high-speed steel developed primarily for high-strength, high-load components (such as bearings and gears) designed for elevated-temperature service. It may be used at temperatures up to 600 F; this is in contrast to AISI 52100 steel which may be...
Journal Articles
Alloy Digest (2001) 50 (12): TS-594.
Published: 01 December 2001
... known to provide good hot hardness, with a hardness of 58.0 HRC under similar conditions. See also Table 1 for hardness values with different hardening and tempering temperatures. Toughness. The toughness of Micro-Melt Maxamet alloy is somewhat lower than that of conventional powder metal high- speed...
Journal Articles
Alloy Digest (1992) 41 (3): TS-510.
Published: 01 March 1992
... CARPENTER MICRO-MELT M-42 alloy is a super-high-speed tool steel produced by powder metallurgy. This production technique results in a more uniform structure, greater ease of grinding, improved wear resistance and toughness than is characteristic of conventionally produced high-speed tool steels...
Journal Articles
Alloy Digest (1996) 45 (11): TS-546.
Published: 01 November 1996
... Carpenter Micro-Melt HS-76 alloy is a superhigh-speed steel made by the powder metallurgy process. The alloy possesses high red hardness, high abrasion resistance, and good toughness. It is proposed for cutting tools where the ASTM M40 series are inadequate. This datasheet provides information on...
Journal Articles
Alloy Digest (1997) 46 (1): TS-549.
Published: 01 January 1997
... Carpenter Micro-Melt T-15 Alloy is a high-speed tool steel made by the powder metallurgy process. The alloy is high carbon with tungsten, cobalt, and vanadium for red hardness and excellent abrasion resistance. Applications include machine tools and cutters. This datasheet provides information on...
Journal Articles
Alloy Digest (2005) 54 (11): TS-622.
Published: 01 November 2005
... Micro-Melt M48 alloy is a superhigh-speed tool steel with a high alloy content and capable of achieving a hardness of 70 HRC. The alloy is used in various tooling and die inserts. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1980) 29 (8): TS-367.
Published: 01 August 1980
... the temperature of the cutting point of the tool in increased greatly. It is well adapted for tools to be used for reaming cast-iron engine cylinders, turning alloy steel or cast iron and cutting nonferrous alloys at high speeds. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1982) 31 (3): TS-395.
Published: 01 March 1982
... hardness, thereby enabling the tool to maintain a higher hardness at elevated temperatures. Type T4 is well adapted for cutting hard, gritty materials such as cast iron or other abrasive materials and for cutting nonferrous alloys at high speeds. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1983) 32 (11): TS-418.
Published: 01 November 1983
... VASCO M-30 is a high-speed tool steel containing nominally 8.70% molybdenum and 4.75% cobalt. It provides long life in machining difficult-to-cut metals, such as heat-resisting alloys and super-alloys. It is recommended for cutting tools requiring a good combination of suitable toughness with...
Journal Articles
Alloy Digest (1970) 19 (4): TS-229.
Published: 01 April 1970
... BRAETUF is a modified version of AISI Type M44 high-speed steel having superior cutting performance and superior wear resistance. It is an ultrahard high-speed steel recommended for machining highly alloyed steels at high hardnesses and also heat teated high temperature alloys. This datasheet...
Journal Articles
Alloy Digest (1961) 10 (12): TS-112.
Published: 01 December 1961
... STAR-M0 M-2 is a tungsten-molybdenum high-speed steel of the 6-6-2 type having good red-hardness quality. This alloy corresponds to AISI type M2. Star-M0 is also available in Free-Machining type, to which sulfur, in the form of alloy sulphides, has been added for better machinability and increased...
Journal Articles
Alloy Digest (1998) 47 (10): TS-561.
Published: 01 October 1998
... Vanadis 23 is a Cr-Mo-W-Va alloyed high-speed steel made by powder metallurgy. The tool steel offers an excellent combination of wear resistance and toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1999) 48 (1): TS-566.
Published: 01 January 1999
... Vanadis 30 is cobalt alloyed high-performance, high-speed steel made by powder metallurgy. The cobalt addition of approximately 8.5% has a positive influence on the hot strength, hot hardness, temper resistance, and modulus of elasticity. Punches are a suitable application for this alloy. This...
Journal Articles
Alloy Digest (2005) 54 (10): TS-620.
Published: 01 October 2005
... Micro-Melt T15 Plus alloy is a high-speed powder metal tool steel. It may be considered for many types of tooling applications where either conventional or powder metal high-speed steels of either the M or T types are being used. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2019) 68 (4): TS-761.
Published: 01 April 2019
... Böhler (or Boehler) S705 is cobalt alloyed, tungsten-molybdenum high-speed steel possessing high hardness, excellent cutting properties, high red hardness, and good toughness. See also Alloy Digest TS-776, September 2019. This datasheet provides information on composition, physical properties, and...