1-20 of 42 Search Results for

SM-200

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1964) 13 (2): Ni-88.
Published: 01 February 1964
... SM-200 is a nickel-base alloy designed primarily as a cast turbine blade material which retains useful strength up to 1900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1962) 11 (6): Co-32.
Published: 01 June 1962
... SM 302 is a cast cobalt-base alloy having superior oxidation and thermal shock resistance. It was designed primarily for use as a first stage turbine vane to operate in the temperature range of 1500-2000 F. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1972) 21 (12): CI-37.
Published: 01 December 1972
... Tensile strength, psi Yield strength, psi Elongation (2 in % Brinell hardness Charpy impact (V-notch), ft-lb Table 1 - TYPICAL MECHANICAL PROPERTIES SM-60-E SMSO-E SM-100-E SM-120-E53QD 60-80000 80-100000 9oooo 100170000 4560000 60-70000 65000 70- 130000 15-25 3-10 1-5 l-5 150-190 200-270 240 260600 7-15...
Journal Articles
Alloy Digest (2009) 58 (12): CS-151.
Published: 01 December 2009
... and sintered at 1120 °C (2050 °F) in 90N2-10H2 (vol Austenitized at 900 °C (1650 °F) and oil quenched, tempered at 200 °C (400 °F). Powder size +250 mm (+60 US SM) 250/+150 mm ( 60/+100 US SM) 150/+45 mm ( 100/+325 US SM) 45 mm ( 325 US SM) Trace 10 65 25 US SM, US Standard Mesh Fig. 1 Hardenability...
Journal Articles
Alloy Digest (2015) 64 (7): SS-1218.
Published: 01 July 2015
... the risks of hot cracking: controlled heat input and travel speed, filler diameter. Recommended filler metals, but not limited to the following: Electrodes: Thermanit 20/16 SM; Fox AM 400 MIG wire: Thermanit 20/16 SM; Fox AM 400 IG Submerged arc: Novonit 3954; Fox AM 500 UP + OP76S Surface Finishing...
Journal Articles
Alloy Digest (1964) 13 (7): Co-38.
Published: 01 July 1964
... alloys joinability machinability oxidation resistance physical properties SM322 tensile properties turbine blades turbine vanes SM 322 Filing Code: Co-38 Cobalt Alloy JULY 1964 -DATA ON WORLD WIDE METALS AND ALLOYS 94 322 (High Temperature Alloy) Psblisbd by Engineering Alloys Digest. Inc...
Journal Articles
Alloy Digest (2016) 65 (10): SS-1253.
Published: 01 October 2016
... after welding. Nitric/hydrofluoric acid mixtures (15% HNO3, 1% HF) can be used between 20 55 °C (68 131 °F). Rinse after pickling. Welding Fillers. Electrodes: Thermanit 20/16 SM Fox AM 400 MIG wire: Thermanit 20/16 SM Fox AM 400 IG Submerged arc: Novonit 3954 Fox AM 500 UP + OP 76S...
Journal Articles
Alloy Digest (1961) 10 (4): Ni-65.
Published: 01 April 1961
..., Annealed Rolled 1300°F/16 Hrs. Aged 1300°F/16 Hrs. Smi* Smax m=l/ smax minzSmax Smin l j2 Smax Smi*=Smax Sm=l/2 S S max 43,000 70,000 40,000 69,000 43,000 68,000 rn 0 35,000 0 34,500 0 34,000 sa 43,000 35,000 40,000 34,500 43,000 34,000 smax = max. Algebraic Stress in Cycle Smin z min. sm = mean stress...
Journal Articles
Alloy Digest (1994) 43 (8): SA-478.
Published: 01 August 1994
.... The precipitations of car- bides are responsible for both the increased resistance to hydrogen attack and creep-rupture strengths. Table 2 - ASM E SECTION VIII YIELD STRENGTH AND DESIGN STRESS INTENSITY VALUES, DIVISION 2 For Metal Yield Design Stress Temperature Strength Intensity Not Exceeding OF Sy, ksi Sm, ksi...
Journal Articles
Alloy Digest (1993) 42 (9): Cu-587.
Published: 01 September 1993
... Minute (Sm): Feed : Feed Per Revolution in inches (FPR) ...
Journal Articles
Alloy Digest (2000) 49 (8): SA-505.
Published: 01 August 2000
... between 1093 and 1149 °C (2000 and 2100 °F). Specification Equivalents: The following list of popular industry specifications is a general reference for this alloy steel and its minor variants. This should not be considered a complete listing. SNECMA. DMD 180-20 Ubra Cuscinetti SM.001 Aerospatile IGC...
Journal Articles
Alloy Digest (1993) 42 (8): SS-548.
Published: 01 August 1993
... of welding filler metals for welding. One is Sumitomo STG 347 AP filler for TIG welding and the other is Sumitomo SM 347 AP filler for MIG welding Sumitomo 347 AP. Table 3 lists their chemical compositions. General Characteristics: Sumitomo 347 AP is a new stainless developed for heat- ing furnace tubes...
Journal Articles
Alloy Digest (1994) 43 (2): Cu-596.
Published: 01 February 1994
... ON .M.IUPHCRY ronhi - SM ON FACE DATA Roughing SFM 400 FPR .005 Semi- SFM 500 Finishing FPR .005 Finishing SFM 750 To 32 RMS FPR .004 Side Rake A See B Diagram Land Rake C Speed, Feed* Same as carbide inserts Rake Type See Diagram Recommended Rough Semi-Finish Finish Grades of Carbide Cut Carbide Cur Carbide...
Journal Articles
Alloy Digest (2015) 64 (6): CS-190.
Published: 01 June 2015
... in the dispersion of fine particles, thus minimizing the inclusion having an influence on cracking initiation. Specification Equivalents: Proprietary SM-125ES. TGP-3166 API 5CT / ISO 11960 NACE MR0175 / ISO 15156-2 API 5C1 / ISO 10405 NACE TM0177 General Characteristics: SM125ES is a low alloy, high strength carbon...
Journal Articles
Alloy Digest (2002) 51 (7): Cu-685.
Published: 01 July 2002
... for soldering Good Capacity for brazing Good Oxyacetylene welding Good Gas-shielded arc welding Good Butt resistance welding Good Seam and spot resistance welding Good Specification Equivalents: UNS C64700 modified ASTM B 411, B 412 EN CuNi2Si, alloy CW111C DIN CuNi2Si, W.Nr. 2.0855 SWISSMETAL® SM 468C...
Journal Articles
Alloy Digest (1989) 38 (11): Ni-376.
Published: 01 November 1989
... proper&z of NICKELVAC901 at room and elevated temperatures. Y SSM sm Y . SW . Y ma TlhlE-)lot;;s - ma- Figure 4 -Stress-rupture life of NICKELVAC-901. Heat Treatment: Solution Treatment: Heat to and hold for 2 hours at 2OOO F (1093 C), air cool or quench (oil or water). Hardness will be about 185 Brinell...
Journal Articles
Alloy Digest (1990) 39 (4): Cp-7.
Published: 01 April 1990
...). Its chemical sm~cture may be represented as follows: PROPERTIES Table 1 -STATIC DATA, DENSlTY AND SFECIFIC HEAT. KEVLUP 49 FIBERS T-Temperature 250°F Axialmodulus*,psix lo (MPax 10) Transverse mod&s*, psi x 106 (MPax l@) AxialsheLarmodulus*,psix106(MPax1~) Axial Poisson sratio* Transverseshearmodulus...
Journal Articles
Alloy Digest (1966) 15 (2): SS-177.
Published: 01 February 1966
... the tensile strength is influenced by different temperatures and times during the tempering of heavily cold rolled austenitic stainless steel (C = 0.14, Si = 1.25, Mn = 1.03, Cr = 18.4, Ni = 8.3, MO = 0.70, N = 0.025 Tensile Sm psi kg/mm* Xlooo 1 425oc / 7@5= F 4OOOC 75O F ,450~C S40°F 475% SWF 114 1 410 50...
Journal Articles
Alloy Digest (2015) 64 (3): CS-185.
Published: 01 March 2015
... the robustness of its material designs and processes. This alloy was successfully tested up to 1000 kPa or 10 bar H2S, and is to be considered full fledge sour service. Specification Equivalents: Proprietary SM-SX Series API 5CT / ISO 11960 NACE MR0175 / ISO 15156-2 API 5C1 / ISO 10405 NACE TM0177 General...
Journal Articles
Alloy Digest (2015) 64 (4): CS-187.
Published: 01 April 2015
.... Specification Equivalents: Proprietary SM-SX Series API 5CT / ISO 11960 NACE MR0175 / ISO 15156-2 API 5C1 / ISO 10405 NACE TM0177 General Characteristics: SM90XS is a low alloy carbon steel OCTG material suitable for severe sour service application. This alloy is a sulfide stress cracking (SSC) resistant...