Skip Nav Destination
Close Modal
Search Results for
SILMO
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1
Search Results for SILMO
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
SILMO: Oxidation Resistant Steel
Available to Purchase
Alloy Digest (1956) 5 (2): SA-38.
Published: 01 February 1956
... SILMO is a silicon-molybdenum, low carbon steel recommended for applications in which a good combination of high temperature strength and oxidation resistance is required. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness...
Abstract
View articletitled, <span class="search-highlight">SILMO</span>: Oxidation Resistant Steel
View
PDF
for article titled, <span class="search-highlight">SILMO</span>: Oxidation Resistant Steel
SILMO is a silicon-molybdenum, low carbon steel recommended for applications in which a good combination of high temperature strength and oxidation resistance is required. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-38. Producer or source: Timken Roller Bearing Company.