Alloy Digest (1985) 34 (10): TS-448.
Published: 01 October 1985
... SELECT B is a fully uniform air-hardening die steel having abrasion resistance intermediate between Olympic (AISI Type D2) high-carbon, high-chromium die steel and Badger (AISI Type O1) oil-hardening die steel. SELECT B has excellent non-deforming, deep-hardening characteristics and good toughness...
Journal Articles
Alloy Digest (1961) 10 (8): TS-108.
Published: 01 August 1961
... Select B FM is a high carbon-medium chromium fully uniform air hardening die steel. It possesses excellent non-deforming properties, is deep hardening and has the balance of toughness and wear resistance required for difficult applications. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2021) 70 (6): Al-477.
Published: 01 June 2021
... and Selection of Aluminum Alloys, Volume 2B, ASM Handbook, ASM International, 2019, p 334. (b) Alloy 3003, Atlas Steels, 2013. (c) For the O temper Mechanical Properties Atlas 3003 is not hardenable by heat treatment. However, it can be significantly strengthened by cold work, enabling httpsdoi.org/10.31399...
Journal Articles
Alloy Digest (2021) 70 (1): Al-472.
Published: 01 January 2021
... condition. (b) T6 = solution heat-treated and then artificially aged. 0.20 0.6 0.20 0.6 (c) Source: Properties and Selection of Aluminum Alloys, Volume 2B, ASM Handbook, ASM International, 2019, p 290 0.20 0.6 0.20 0.6 0.05 0.05 0.15 0.15 Mechanical Properties See Tables 1 and 2. bal bal Corrosion...
Journal Articles
Alloy Digest (2021) 70 (11): Al-482.
Published: 01 November 2021
... from Properties and 0.05 0.05 Selection of Aluminum Alloys, Volume 2B, ASM Handbook, ASM International, p 348. 0.15 0.15 Hot Forming bal bal Heat to 510 °C (950 °F). Wait for equalization of the tempera- (a) Maximum values unless indicated otherwise. (b) Source: ASTM B209:2014 and ture. Do not finish...
Journal Articles
Alloy Digest (2020) 69 (11): Al-470.
Published: 01 November 2020
... a pleasant matte finish. Chemical Composition Element Silicon Iron Copper Manganese Magnesium Chromium Zinc Others, each Others, total Aluminum Composition, wt%(a) Atlas 5052 Alloy 5052 (UNS A95052)(b) 0.25 0.25 0.40 0.40 0.10 0.10 0.10 0.10 2.2 2.8 2.2 2.8 0.15 0.35 0.15 0.35 0.10 0.10 0.05 0.05 0.15 0.15...
Journal Articles
Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... Carbon CP Grade 7 Titanium (UNS R52400)(b) Electrical m 0.42 0.52 resistivity circular- (253 313)(c) 0.08 0.08 mil/ft) Oxygen 0.25 0.25 RT = room temperature. (a) Titanium Alloy Guide, RMI Titanium Company, 2000, p.19. (b) Source: Properties and Selection: Nonferrous Alloys and Special-Purpose Materials...
Journal Articles
Alloy Digest (1985) 34 (9): TS-446.
Published: 01 September 1985
... VISCOUNT 20 is an air-hardening, 5% chromium hot-work steel with the same analysis as Latrobe's VDC except for the addition of carefully controlled and evenly dispersed alloy sulfides. These additives improve the machinability of the steel so that it is an excellent selection for a variety of hot...
Journal Articles
Alloy Digest (2021) 70 (6): Ni-772.
Published: 01 June 2021
...: Properties and Wire diameter Rm(b), min A(c) Selection: Nonferrous Alloys and Special-Purpose Materials, Volume 2, ASM Handbook, % ASM International, 1990, p 834 mm in. MPa ksi 14 14 0.063 0.125 0.0025 0.0049 650 94.3 18 25 > 0.125 0.5 > 0.0049 0.0197 to oxide scaling and to thermal...
Journal Articles
Alloy Digest (2022) 71 (3): Al-486.
Published: 01 March 2022
... and permanent mold castings. It is a high-strength alloy with many desirable characteristics. The presence of copper in alloy 355.0 increases strength but reduces corrosion resistance and ductility. This alloy is less ductile than 356.0. Chemical Composition Element Alloy 355.0(b)(c) Composition, wt%(a) Alloy...
Journal Articles
Alloy Digest (2021) 70 (3): Al-474.
Published: 01 March 2021
...) (a) Primary Aluminum Foundry Alloys, Rio Tinto, 2019, p 17. (b) Properties and Selection of Aluminum Alloys, Volume 2B, ASM Handbook, ASM International, 2019, p 533. (c) For sand castings Physical Properties Mechanical Properties See Tables 1, 2, and 3. Property Unit At Value Corrosion Resistance Liquidus °C...
Journal Articles
Alloy Digest (2020) 69 (2): Cu-905.
Published: 01 February 2020
.... (a) Calculated value Fig. 1 Comparison of yield strength and electrical conductivity performance of select automotive connector materials. Table 1 Mechanical properties Temper designation(a) Tensile strength Yield strength(b) Elongation(b)(c) Typical bend radius (90° bend) (b)(d) Standard Former MPa ksi MPa ksi...
Journal Articles
Alloy Digest (2022) 71 (10): Al-490.
Published: 01 October 2022
...) 152 (88)(a) 963 (0.230) 0.0479 (29)(a) 21 (36)(a) (a) For alloy 355.0 sand castings in the T6 temper. Source: 355.0 and C355.0: Al-Si-Cu High-Strength Casting Alloys, Properties and Selection of Aluminum Alloys, Volume 2B, ASM Handbook, ASM International, 2019, p 544 Mechanical Properties See Tables 1...
Journal Articles
Alloy Digest (1980) 29 (1): CI-49.
Published: 01 January 1980
... ABEX PARABOLOY is a high-chromium cast iron produced under strictly controlled foundry conditions and heat treated to furnish two grades: PAB and PAC. PAB provides excellent wearlife in heavy-section castings for mill liners and selected crusher parts. PAC provides excellent service...
Journal Articles
Alloy Digest (2020) 69 (12): Ni-765.
Published: 01 December 2020
... Manganese Silicon Phosphorus Sulfur Chromium Molybdenum Tungsten Aluminum Lanthanum Cobalt Titanium Boron Iron Copper Nickel Composition, wt%(a) ATI 6230 UNS N06230(b) 0.05 0.15 0.05 0.15 0.30 1.00 0.30 1.00 0.25 0.75 0.25 0.75 0.030 0.030 0.015 0.015 20.0 24.0 20.0 24.0 1.0 3.0 1.0 3.0 13.0 15.0 13.0 15.0...
Journal Articles
Alloy Digest (1996) 45 (5): Ni-12.
Published: 01 May 1996
... CHLORIMET 2 is a nickel-base alloy that provides good resistance to corrosive conditions not normally handled by other types of commercially available alloys. CHLORIMET 2 is a refined equivalent of HASTELLOY B and is most commonly used in engineered equipment, such as pumps and valves, made...
Journal Articles
Alloy Digest (2021) 70 (8): Al-479.
Published: 01 August 2021
...) 0.05 0.05 0.05 963 0.15 0.15 0.15 (0.230) bal bal bal 18.6 (32) (a) Maximum values unless indicated otherwise. (b) The digit to the right of the deci- mal point indicates the product form: 0 denotes castings, 1 denotes standard ingot, and Source: Properties and Selection of Aluminum Alloys, Volume 2B...
Journal Articles
Alloy Digest (2000) 49 (1): Al-366.
Published: 01 January 2000
... (a) Notch fatigue factor of 3.0. Source: Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, Vol 2, ASM Handbook, ASM International, 1990, p 113 Table 2 Comparative Characteristics Corrosion resistance Weldability(d) Temper General(a) Stress(b) Cold workability(c) Machinability(c...
Journal Articles
Alloy Digest (2020) 69 (1): Cu-903.
Published: 01 January 2020
... Mechanical Properties See Tables 1 and 2. A comparison of yield strength and electrical conductivity performance of select hard temper copper-based materials is shown in Fig. 1. Comparable Grades ASTM SAE UNS C10200 UNS C10200 ISO EN Cu-OF (CW008A) JIS C 1020 General Characteristics Excellent hot and cold...
Journal Articles
Alloy Digest (1965) 14 (8): TS-168.
Published: 01 August 1965
... A-2 Sparta Ry-Die Airkool Select B Carpenter 484 Sagamore Bethlehem AH-5 Air Hard Airvan General Characteristics: Universal Cyclops Ryerson Crucible Lanobe Carpenter Allegheny Ludlum Bethlehem Vanadium Alloys Fir& Sterling AISI Type A2 is an air hardening cool and die steel intermediate in abrasion...