Skip Nav Destination
Close Modal
Search Results for
SD 170
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3 Search Results for
SD 170
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (9): W-28.
Published: 01 September 2005
... elasticity hardness physical properties SD 170 SD 175 SD 180 SD 185 tensile properties workability Chemical Composition, wt (Nominal) SD 170 SD 175 SD 180 SD 185 Tungsten 90 92.5 95 97 Nickel 7.1 5.4 3.6 2.1 Iron 2.9 2.1 1.4 0.9 Physical Properties: (Typical) Density, kg/m3 (lb/in.3 ) SD 170...
Abstract
View article
PDF
The SD group is part of the Densalloy family of materials, which are high-density alloys used for a variety of applications, from counterbalance weights to radiation shielding. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming. Filing Code: W-28. Producer or source: Tungsten Products, An Allegheny Technologies Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1956) 5 (3): TS-44.
Published: 01 March 1956
... screw sto& Carbide-tipped cutting tools should be designed for 6 deg side reIief angie, 6 deg. side rake a&. 8 12 deg. end cutting-edge angle and side cuaing-edge angle, 6 deg. end relief angie, 2 deg. back rake a~gk. High speed .sd lathe tools should have a nose radius qud to 10% of cut depth...
Abstract
View article
PDF
CROCAR is an air or oil hardening high-carbon high-chromium die steel having extreme wear and abrasion resistance. It is equivalent to AISI Type D4 and ASM Class IID-3. This datasheet provides information on composition, hardness, and compressive strength as well as deformation. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-44. Producer or source: Vanadium Alloys Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (3): SS-403.
Published: 01 March 1982
... Property At 68 F At 212OF At 392OF Tensile strength, MPa Yield strength (0-g offset), MPa Yield strength (1.0% offset), ga Elongation (SD), % Hardness, DPH (Vidcers) Brinell hardness 600800 87000-116000 300 43500 340 49500 40 180 170 230 190 33500 26500 260 230 38000 33500 8.0 0.293 1400 (2550) 0.; 1s x 10...
Abstract
View article
PDF
CRONIFER 1925 HMo is an austenitic chromium-nickel-molybdenum stainless steel. The high contents of chromium and especially molybdenum make this steel highly resistant to pitting and crevice corrosion. Because of its high nickel content, its resistance to stress-corrosion cracking is considerably higher than that of the common austenitic stainless steels. CRONIFER 1925 HMo has good strength and ductility, high impact values and good weldability. Its applications include heat exchangers for use with salt water, bleaching-plant equipment and flue-gas scrubbers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-403. Producer or source: Vereingte Deutsche Metallwerke AG.