1-2 of 2 Search Results for

SARATOGA

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1976) 25 (8): TS-306.
Published: 01 August 1976
... SARATOGA is an oil-hardening tool steel combining a strong and tough cutting edge with great freedom from shrinking and warping. It is recommended for a wide range of tool-room requirements. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1955) 4 (9): TS-38.
Published: 01 September 1955
... important to allow the steel to become black after completion of the forging hefore charging into the nor- malizing furnace. Specification Equivalents: Saratoga (Allegheny Ludlum) BTR (Bethlehem) Kiski (Braeburn) EXLDie (Columbia) Kctos (Crucible) Mansil (Disston) Invaro No. 1 (Firth Sterling) Truform...