1-2 of 2 Search Results for

SANDVIK SANICRO 63

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2001) 50 (8): Ni-572.
Published: 01 August 2001
... Sandvik Sanicro 63 was developed specifically for use as outer cladding of composite tubes in service as superheater materials for waste-derived fuel plants. It is a modification of UNS N06625. Typical inner components of the composite tubes are Sandvik 4L7 and Sandvik HT8. This datasheet provides...
Journal Articles
Alloy Digest (1992) 41 (4): SS-526.
Published: 01 April 1992
... is also excellent. *Sandvik, SAF 2507 and Sanicro are trademarks of Sandvik AEL Chemical Composltion (Nominal): Carbon 0.03 max. Silicon 0.8 max. Manganese 1.2 max. Phosphorus 0.035 max. SU1ft.U 0.02 max. Chromium 25 Nickel 7 Molybdenum 4 Nitrogen 0.3 Iron Remainder. Temperature. C (OFI 30 (85) Physical...