Alloy Digest (2019) 68 (7): SS-1307.
Published: 01 July 2019
... (302 °F) 13 (7.5) 200 °C (392 °F) 14 (8.1) 250 °C (482 °F) 15 (8.7) 300 °C (572 °F) 16 (9.2) Copyright © 2019, ASM International®. All rights reserved. SANDVIK SANICRO 28 for OCTG (Nitriding Steel) Filing Code: SS-1307 Stainless Steel :: July 2019 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax...
Journal Articles
Alloy Digest (1984) 33 (3): SS-442.
Published: 01 March 1984
... SANDVIK Sanicro 28 is an all-purpose low-carbon stainless steel alloy for service in highly corrosive environments. It has exceptionally high resistance to various types of corrosive attack and has good weldability. Among its numerous applications are evaporator tubes in the production...
Journal Articles
Alloy Digest (2001) 50 (9): SS-831.
Published: 01 September 2001
... Sandvik Sanicro 28 composite tube is used in services as superheater material for waste-derived fuel plants. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2014) 63 (3): SS-1169.
Published: 01 March 2014
... Sandvik Sanicro 29 is a corrosion resistant grade (CRA) available as seamless product heavily cold worked for oil country tubular applications at high strengths. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2018) 67 (9): SS-1293.
Published: 01 September 2018
...) 210 (30.5) 520 (75) 600 (1112) 180 (26) 205 (30) 500 (72.5) 650 (1202) 180 (26) 210 (30.5) 480 (70) 700 (1292) 180 (26) 195 (28) 455 (66) 750 (1382) 180 (26) 195 (28) 410 (59) 800 (1472) 180 (26) 195 (28) 355 (51.5) Table 2 Creep properties of Sandvik Sanicro 25 Temperature, °C (°F) Creep properties...
Journal Articles
Alloy Digest (2017) 66 (11): Ni-739.
Published: 01 November 2017
... Sandvik Sanicro 72HP is a corrosion- and oxidation-resistant grade (CRA) available as wire, particularly weld wire. Sanicro 72HP is commonly used as weld wire for joining NiCrFe alloys. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1996) 45 (8): SA-483.
Published: 01 August 1996
... Sandvik Sanicro 38/4L7 is a composite tube consisting of Sanicro 38, a corrosion-resistant nickel-base alloy on the outside diameter, and carbon steel (A210 GrA-1) for water-wetted service on the inside. The design is placed entirely on the inside tube; however, there is a contribution from both...
Journal Articles
Alloy Digest (1992) 41 (4): SS-526.
Published: 01 April 1992
... is also excellent. *Sandvik, SAF 2507 and Sanicro are trademarks of Sandvik AEL Chemical Composltion (Nominal): Carbon 0.03 max. Silicon 0.8 max. Manganese 1.2 max. Phosphorus 0.035 max. SU1ft.U 0.02 max. Chromium 25 Nickel 7 Molybdenum 4 Nitrogen 0.3 Iron Remainder. Temperature. C (OFI 30 (85) Physical...
Journal Articles
Alloy Digest (1965) 14 (12): Ni-108.
Published: 01 December 1965
... Sanicro 71 is a nickel-base alloy having good resistance to stress-corrosion, oxidation and creep at elevated temperatures. It is recommended for nuclear power reactor heat exchanger tubes, aircraft turbojet engines and for equipment in the textile, plastic, and chemical industries. This datasheet...
Journal Articles
Alloy Digest (1989) 38 (8): SS-267.
Published: 01 August 1989
... are recommended for TIG and MIG welding in cases where there is a risk of weld metal stress cracking. For manual metal-arc welding. use Sandvik 29.9R. 25.20R or Sanicro 72. Corrosion Resistance: Sandvik 4C54 is resistant to oxidation at constant and cyclical varying temperatures. The limiting service temperature...
Journal Articles
Alloy Digest (2004) 53 (7): Ni-622.
Published: 01 July 2004
... 100 338 49.0 68 Table 2 Comparative Corrosion Resistance Corrosion rate, average, mils/yr Media G-35 G-30 Sanicro 28 65% nitric acid, boiling 2.8 3.6 2.3 10% hydrofluoric acid, 52 °C (125 °F) 7.5 22.7 66.2 10% sulfuric acid, 93 °C (200 °F) 0.2 0.2 41.2 50% sulfuric acid, 66 °C (150 °F) 0.1 0.2 11.4 5...
Journal Articles
Alloy Digest (1997) 46 (11): SS-699.
Published: 01 November 1997
...- mends wire electrodes and rods Sandvik 72. In manual metal-arc welding covered ekcmdes Sandvik Sanicro 72 are recom- mended. For application at temperatures up to 400 C (750 m. welding wire/d Sandvik 19.9.NbSi. 19.9.Nb. 19.9.LSi or 19.9.L and covered electmdes Sandvik 19.9.NbR or 19.9LR are recommended...
Journal Articles
Alloy Digest (2001) 50 (1): SS-812.
Published: 01 January 2001
... is somewhat impaired. For service in this temperature range, the producer recommends the use of Sandvik Sanicro 31HT (see Alloy Digest SS-643), which has better struc- tural stability. Maximum service temperature in air is 1100 °C (2010 °F). Product Forms Available: Seamless tube and pipe are generally...