Alloy Digest (1987) 36 (7): SS-487.
Published: 01 July 1987
... SANDVIK SAF 2205 is an extra-low carbon, ferritic-austenitic stainless steel. It has high resistance to stress-corrosion cracking; pitting; service and general corrosion. It has roughly twice the yield strength of austenitic stainless grades and it has good weldability. This datasheet provides...
Journal Articles
Alloy Digest (2015) 64 (2): SS-1203.
Published: 01 February 2015
... Sandvik SAF 2205 PM is a duplex (austenitic/ferritic) stainless steel made by hot isostatic pressing a powder. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion...
Journal Articles
Alloy Digest (2011) 60 (7): SS-1097.
Published: 01 July 2011
... Sandvik Sanmac SAF 2205 (a Sandvik hollow bar material) is a duplex ferritic/austenitic stainless steel grade in hollow bar that meets the chemical requirements of WNr. 1.446, SAF 2205 and UNS S31803, but has improved machinability. Recommendations on cutting are given on machining with modern CNC...
Journal Articles
Alloy Digest (1996) 45 (9): SS-652.
Published: 01 September 1996
..., crevice. and general corrosion; it has a very high resistance to chloride stress-cormsion cracking. SAF 2507 is a registered trademark of Sandvik AB. 2205 Code Plus Two is a registered takmark of Avesta AB Chemical Composition, wt Nomrrml Asnm cabm 0.020 0.030IIrax. 25.0 24.IH6.0 iiz$LBm 4.0 7 6.G8.0...
Journal Articles
Alloy Digest (1996) 45 (8): SS-649.
Published: 01 August 1996
... in chloride solutions. One method is to determine the temperanne above which pitting is initiated. the critical pitting tempemmre (CFT). The CPT of Avesta Sheffield SAF 2304 is comparable to that of Type 316L and superior to that of Type 304L. The CPT of Avesta Sheffield 2205 Code Plus Two@ steel is higher...
Journal Articles
Alloy Digest (2004) 53 (5): SS-903.
Published: 01 May 2004
... S32304 DIN 1.4362, S2CrNiN23L) Sandvik SAF 2304 Industeel UR35N. Product Forms Available: Supermet 2205 is available in the size, weight, and pieces shown in Table 4. Applications: Supermet 2205 and wrought duplex austenitic/ferritic stainless steels are increasingly used in the offshore oil/gas...
Journal Articles
Alloy Digest (2005) 54 (8): SS-936.
Published: 01 August 2005
..., it is rec- ommended that the austenitic-ferritic steels Sandvik SAF 2304, Sandvik 10RE51, or Sandvik Sanmac SAF 2205 be used. Pitting and Crevice Corrosion. The steel may be sensitive to pitting and crevice corrosion even in solutions of relatively low chloride content. Molybdenum-alloyed steels have better...
Journal Articles
Alloy Digest (2006) 55 (11): SS-981.
Published: 01 November 2006
.... SAF 2507 is a registered trademark of Sandvik AB. See Table 1. The range of use for this alloy is 50 to 270 °C ( 58 to 518 °F). Heat Treatment: This alloy is delivered in the solution-annealed and water-quenched condition, with treatment at 1080 1120 °C (1976 2048 °F). The chemical analysis and heat...
Journal Articles
Alloy Digest (2000) 49 (11): SS-777.
Published: 01 November 2000
... down must also be considered, as the conden- sates that are then formed can develop a chloride content that leads to both stress-corrosion cracking (SCC) and pitting. In applications demanding high resistance to SCC, austenitic-ferritic steels such as Sandvik SAF 2304 or SAF 2205 are recommended. Gas...
Journal Articles
Alloy Digest (2001) 50 (7): SS-465.
Published: 01 July 2001
.... It is significantly stron- ger than most low-carbon stainless steels and its structural stability makes for good weldability. AvestaPolarit, 254 SMO, 654 SMO, and 2205 Code Plus Two are registered trademarks of AvestaPolarit AB. SAF 2304 and SAF 2507 are trademarks of AB Sandvik Steel. Chemical Composition, wt Carbon...