Alloy Digest (2000) 49 (6): SS-793.
Published: 01 June 2000
... Sandvik Bioline High N is a molybdenum-alloyed stainless steel for implant applications. Corrosion resistance to physiological environments is good. The alloy is of high purity and has an excellent surface finish. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2000) 49 (5): SS-784.
Published: 01 May 2000
... implantable medical devices. Producer: Sandvik Steel Company Tubular Products Division Scranton, PA 18501-1220 (570) 585-7511 (570) 585-7513 (fax) In Sweden: Sandvik Steel Sandviken +46 26-26 30 00 +46 26-25 17 10 (fax) ISSN: 002-614X SS-784B Temperature °F °C 210 100 175 80 140 60 105 40 7 20 316LVM High-N...
Journal Articles
Alloy Digest (2011) 60 (9): SS-1102.
Published: 01 September 2011
... Sandvik Bioline 7C27 an alloy that hardens well and has good corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming and heat treating. Filing Code: SS-1102. Producer or source...