1-2 of 2 Search Results for

SANDVIK BIOLINE 316LVM

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2000) 49 (5): SS-784.
Published: 01 May 2000
... Sandvik Bioline 316LVM is a molybdenum-alloyed stainless steel for implant applications. Corrosion resistance to physiological environments is good. The alloy is of high purity and has an excellent surface finish. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2000) 49 (6): SS-793.
Published: 01 June 2000
...: Sandvik Bioline stainless implant steels are used to manufacture bone screws, compression plates, intra-medullar nails, interlocking DOI: 10.31399/asm.ad.ss0793 Temperature °F °C 210 100 175 80 140 60 105 40 7 20 316LVM High-N Fig. 1 Critical pitting temperature (CPT), potentiostatic determination...