1-1 of 1 Search Results for

SANDVIK 8R40

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1995) 44 (4): SS-590.
Published: 01 April 1995
... SANDVIK 8R40 is an austenitic, columbium stabilized stainless chromium-nickel steel for use at temperatures up to 850 C (1560 F). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on...