... Sandvik 8R30 is an austenitic, titanium-stabilized stainless chromium-nickel steel. It is suitable for wet-corrosive service, but also has good mechanical strength at high temperatures. For applications requiring enhanced creep strength, it is recommended that the variant Sandvik 8R30H be used...