Alloy Digest (1997) 46 (11): SS-699.
Published: 01 November 1997
... SANDVIK 6R35 is an austenitic titanium stabilized chromium nickel steel with good mechanical strength at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also...