Alloy Digest (1996) 45 (7): SA-482.
Published: 01 July 1996
... Sandvik 3R12/4L7 is a composite tube consisting of type 304L stainless steel for corrosion resistance on the outside diameter and having carbon steel (A210 Gr. A1) as the inside component for both water wetted service and the design load. The major application is tubing to handle the corrosive...