Alloy Digest (2011) 60 (2): Ni-687.
Published: 01 February 2011
... Sandmeyer alloy 825 is a nickel alloy high in chromium and molybdenum with good corrosion resistance and ductility. The alloy has enough nickel (42%) to be relatively free from chloride-ion stress-corrosion cracking. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2008) 57 (7): SS-1016.
Published: 01 July 2008
... temperatures is good for austenitic steel. In pure sulfuric acid, it performs significantly better than Type 316L and somewhat better than 904L. Its performance is comparable to the more costly nickel- base materials Alloy 20 and Alloy 825. In phosphoric acid process streams that contain halide impurities, the...