1-20 of 28 Search Results for

SAE 1065

Sort by
Journal Articles
Alloy Digest (2023) 72 (2): CS-240.
Published: 01 February 2023
... hardness heat treatability joinability machinability physical properties S65C tensile properties thermal properties wear resistance workability UNS G10650 UNS G10640 SAE 1064, SAE 1065, ISO CS65, JIS S65C STEEL DATA SURVEY (Wrought High-Carbon Non-Alloy Steels) Filing Code: CS-240 Carbon...
Journal Articles
Alloy Digest (1988) 37 (1): CS-118.
Published: 01 January 1988
... SAE 1065 is a high-carbon oil-hardening machinery and tool steel of low hardenability. It is used for springs, hand tools, machinery parts, shafts and many machine tools requiring strength and wear resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1976) 25 (10): CS-63.
Published: 01 October 1976
... resistant to alkalis at ordinary temperatures. Specification Equivalents: SAE 1065. QQ-S-633. QQS-00640 (Army Ord). General Characteristics: Because of its low hardenability, AISI 1065 can be hardened fully by oil quenching only in very thin sections. Only partial hardening can be achieved in heavier...
Journal Articles
Alloy Digest (1991) 40 (4): Al-315.
Published: 01 April 1991
... 443 is improved corrosion resistance. Spscification Equivalents: AA (C443.1). Federal QQ-A-591F (C443.1), QQ-A-371F (C443.1) ASTM B-85 (S5C) SAE 304 General Chzwacteristks: At a 456.0% silicon content range, Ahrminum Alloy 443 has a somewhat broadened solidikation range. Ma- chinability is also...
Journal Articles
Alloy Digest (1957) 6 (9): Al-56.
Published: 01 September 1957
... to corrosion under both ordi- nary atmospheric and marine conditions. Its resistance may be increased considerably by anodic treatment. Specification Equivalents: Aluminum Association Alloy 13 ASTM B179 Alloy S12A ASTM B85 Alloy S12A Fed. w-A-591-2 Cl. 1 AN-A-38 Alloy 13 Navy 46A14 Cl. 1 SAE 305 British B51490...
Journal Articles
Alloy Digest (1967) 16 (8): Al-168.
Published: 01 August 1967
... severe condi- [ion, but exposures of this rype should be approached with caution. Specification Equivalents: ASTM B85 Alloy S12A Fed. QQ-A-591 Cl. 2 SAE 305 AMS 4292 General Characteristics: Aluminum .413 is similar to Aluminum 13 alloy wirh impurities more closely controlled. It has the same general...
Journal Articles
Alloy Digest (2010) 59 (5): SS-1065.
Published: 01 May 2010
..., J92613 ASTM A 297 (HC); A 608 (HC 30); and A743 (CC50) SAE 70446 Nearest wrought grade: AISI 446. The composition of the wrought grade differs from that of the cast alloy and has different properties. The cast alloys designation should always be used to identify castings. General Characteristics: HC...
Journal Articles
Alloy Digest (1977) 26 (12): Al-231.
Published: 01 December 1977
...); Federal QQA-591d, 413.0 (13); AMS 4292. Ingots: AA No. 413.2 (Former de&nation 13): ASTM B 179. 413.2 (S12AB and S12c); SAE 413.12 (305); QQ-A-371e, 413.2 (13). Sand Castings: AA No. 413.0 (Former designation 13). Permanent-Mold Castings: AA No. 413.0 (Former designation 13). General Characteristics...
Journal Articles
Alloy Digest (2021) 70 (7): SS-1337.
Published: 01 July 2021
... on automatic screw machines at about 70% of the speed of SAE 1212. This sulfur modification has led to widespread acceptance and use of this grade in the screw machine industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2020) 69 (2): Ni-756.
Published: 01 February 2020
... performance is similar to other high-temperature, nickel-base alloys. Copyright © 2020, ASM International®. All rights reserved. Special Precautions All lubricants or coolants, particularly sulfur-bearing fluids, should be removed prior to heat treating and welding. Comparable Grades ATI ASTM SAE ISO EN JIS...
Journal Articles
Alloy Digest (1993) 42 (10): Cu-590.
Published: 01 October 1993
...) Typical softening temperature: 355°C (675°F) Weldability: Soldering - excellent Brazing and resistance butt welding - good Gas-shielded arc welding - fair Oxyacetylene, coated metal-arc and resistance spot and seem welding - not recommended. Specification Equivalents: ASTM See Table 1 SAE bar, plate...
Journal Articles
Alloy Digest (1976) 25 (2): Al-221.
Published: 01 February 1976
... Castings: AA No. 413.0 (Former designation 13). Die Castings: AA No. 413.0 (Former designation 13); ASTM B 85, 413.0 (S12A); SAE 413.0 (305); Federal QQ-A-591d, 413.0 (13); AMS 4290F. Ingots: AA No. 413.2 (Former designation 13); ASTM B 179, 413.2 (S13AB and S12C); SAE 413.2 (305); QQ-A-371e, 413.2 (13...
Journal Articles
Alloy Digest (2021) 70 (2): TS-809.
Published: 01 February 2021
.... Do not finish below 815 °C (1500 °F). Nickel 0.25 Cool in still air. Information on hot forming derived from G. Copper 0.025 0.030 Roberts, G. Krauss, and R. Kennedy, Tool Steels, 5th ed., ASM Vanadium International, 1998, p128, and SAE J437:2018. Tungsten 0.025 0.030 Iron Heat Treatment...
Journal Articles
Alloy Digest (1962) 11 (5): Al-114.
Published: 01 May 1962
... ate the aluminum-magnesium alloys, it is much superior in mildly acid solutions such as ate encounteteJ in the textile industry. Specification Equivalents: Sand Cast Aluminum 43 ASTM B26 alloy SSA % SSB SAE 35 Fed. QQ-A-601 Cl. 2M Permanent Mold ASTM B108 Alloy SSA % SSB SAE 35 Fed. QQ-A-596 Cl. 7 Die...
Journal Articles
Alloy Digest (1958) 7 (10): Al-71.
Published: 01 October 1958
... of the zinc content which is higher in z-39: ASTM B85, AIIoy SC84A at SC84B SAE 306 i-2 308 Federal QQ-A-591, classes 10 at 11 MIL-A-15153a, Class 10 AMS 4291 General Characteristics: An excellent all purpose die casting alloy. No appreci- able reduction in the properties of the alloy occurs until...
Journal Articles
Alloy Digest (1958) 7 (11): Al-72.
Published: 01 November 1958
... Specification Equivalents: ASTM B85 Ahoy S12B SAE 305 Fed. QQ-A-591a-2, Comp. 1 MIL-A-15153a Cl. 1 MIL-A-8294 Comp. 1 ASTM B179-S12 A & B (Ingot) British 1490.LM-20 Canada HA 9.160 France BNP (A-513) General Characteristics: Aluminum 13 is a high-silicon aluminum alloy used mostly for large and complex-shaped...
Journal Articles
Alloy Digest (1990) 39 (8): SS-514.
Published: 01 August 1990
... (3 16) and others. ASTM Al67 (316), Al82 (316), Al93 (316), Al94 (316), A213 (316) andothers. Fed. QQ-S-763 (316), QQ-S-766 (316). QQ-W423 (316) M&S-862 (316), S-5059 (316), S-7720 (316) SAE J405 (30316) General Characteristics: UNS S3 1600 steel is an austenitic stainless with enhanced corrosion...
Journal Articles
Alloy Digest (2021) 70 (5): TS-813.
Published: 01 May 2021
... mm (1 in.) of maximum section thickness. The solution heat treatment temperature must be monitored by a thermo- Carpenter Technology Corporation UNS K92580 couple attached to the load. USA SAE AMS 6532H:2018 3.1Cr-11.5Ni-13.5Co-1.2Mo (0.21- Quenching. CarTech AerMet-for-Tooling is an air hardening...
Journal Articles
Alloy Digest (1984) 33 (5): Al-251.
Published: 01 May 1984
... temperature present a less severe condition. but exposures of this type should be approached with caution. Specification Equivalents: ASTM B 85. Federal QQ-A-59 I. UNS No. A14130. SAE: 5452 and 5453. General Characteristics: Aluminum A413.0 is similar to Aluminum 413.0 except that its iron content is lower...
Journal Articles
Alloy Digest (1964) 13 (4): Al-136.
Published: 01 April 1964
... cakes place and properties are restored wichio three weeks. Specification Equivalents: ASTM B177 Alloy ZGGIB (ingots) ASTM B26 Alloy ZGGIB (sand castings) SAE 313 (J-453) Fed. QQA-371 Comp. X (ingots) Fed. QQ-A-601 Alloy A612 (sand castings) (The designations shown relate eo similar chemical...