Skip Nav Destination
Close Modal
Search Results for
SAE 1060
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-14 of 14 Search Results for
SAE 1060
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (4): CS-220.
Published: 01 April 2022
... International® 2022 2022 ASM International 1059 1060 C60 C60E C60R castability chemical composition corrosion-resistant alloys elasticity formability hardness heat treatability joinability machinability physical properties tensile properties thermal properties UNS G10600 SAE 1059, SAE...
Abstract
View article
PDF
1059, 1060, C60, C60E, and C60R are wrought high-carbon non-alloy steels that are used in the normalized, cold worked, quenched and tempered, or austempered condition. 1059, 1060, C60E, and C60R may also be flame or induction hardened. These steels are widely used for moderately and highly stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and where the expense of an alloy steel is not justified. They are also used for applications where the higher carbon is needed to improve wear characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: CS-220. Producer or source: Data Survey.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1987) 36 (12): CS-116.
Published: 01 December 1987
... SAE 1060 is a high-carbon steel of low hardenability; it may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the desired properties. It is normally hardened by austenitizing and quenching in oil; however, it may be quenched in water...
Abstract
View article
PDF
SAE 1060 is a high-carbon steel of low hardenability; it may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the desired properties. It is normally hardened by austenitizing and quenching in oil; however, it may be quenched in water if precautions are taken to prevent cracking. Its many uses include springs, hand tools, heavy machinery parts, shafts and agricultural machinery. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-116. Producer or source: Carbon steel mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (2): CS-92.
Published: 01 February 1983
... are present. the corrosion rate is increased. The steel is attacked readily by acids. but is somewhat resistant to alkalies at ordinary temperatures. Specification Equivalents: SAE 1060. UNS No. Gl0600. Federal: QQ-S-633 and QQ-S-00640 (Army Ord). Military: MIL-S-16788 and MIL-S-16974. General Characteristics...
Abstract
View article
PDF
AISI 1060 is a high-carbon steel of low hardenability; it may be used in the as-rolled, annealed, normalized or liquid-quenched-and-tempered condition, depending on the desired properties. It is normally hardened by austenitizing and quenching in oil; however, it may be quenched in water if precautions are taken to prevent cracking. Its many uses include springs, hand tools, heavy machinery parts, shafts and agricultural machinery. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-92. Producer or source: Carbon steel mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (3): CS-129.
Published: 01 March 1991
... are only moderately satisfactory. Specification Equivalents: AMS 7240. SAE J408(1060). J412(1060). J414(1060) UNS No. Cl0600 Federal: QQ-S-633 and QQ-S-00640 (Army Ord). Military: MIL-S-16974(Gr1060) AIS1 1060, ASTM A29( 1060). A5 lO( 1060). A576( 1060). A682( 1060). General Characteristics: UNS No. Cl0600...
Abstract
View article
PDF
UNS No. G 10600 is a high-carbon steel of low hardenability. It may be used in the as-rolled, annealed, normalized or quenched and-tempered condition, depending on the desired properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-129. Producer or source: Carbon steel mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (10): SA-62.
Published: 01 October 1957
... weldability with weld metal strength and ductiliry equal to or greater than the parent metal. Specification Equivalents: Proposed SAE Aeronautical Material Speci&ation for billets, bars, rods, wire, shapes, and extrusions. Proposed SAE-AhG-for sheet, strip and plate. General Characteristks: The strength...
Abstract
View article
PDF
VASCOJET 1000 is a 5% chromium steel designed for parts requiring maximum levels of strength, ductility, toughness, fatigue resistance and thermal stability for operation between -100 F and 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-62. Producer or source: Vanadium-Alloys Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (4): Al-25.
Published: 01 April 1955
... Equivalents: Federal QQ-A-367 Cl. 6 Navy 46A7 Cl. 6 SAE 290 AMS 4145 ASTM B247 AUoy SG 121A General Characteristics: AI.Uh!UNUM 4032 was formerly known as Alcoa 32s and Alu.@nium 32s alloy. It is high silicon forging alloy with low co&&m of expansion and good cor- rosion resistance. It has exceilenc...
Abstract
View article
PDF
ALUMINUM 4032, formerly known as Aluminium 32S, is a forging alloy having comparatively low coefficient of expansion and good forgeability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as creep and fatigue. It also includes information on low and high temperature performance as well as heat treating, machining, and joining. Filing Code: Al-25. Producer or source: Aluminum Company of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (1): Al-249.
Published: 01 January 1984
... to prevent the development of welding cracks due to the quick chill of the weld. Specification Equivalents: ASTM B 26. UNS No. A07120. Federal: QQ-A-601 and QQ-R-566. SAE 5452 (310) and 5453 (310). Military: MIL-C- 11866 (40E) and MIL-F-39OOO(D712.0). General Characteristics: Aluminum 712.0 is a high...
Abstract
View article
PDF
ALUMINUM 712.0 is a high-strength aluminum casting alloy that is self aging at room temperature. It has good machinability, good dimensional stability and good resistance to corrosion and shock. Among its applications are marine castings, high-strength pressure-tight castings, aircraft components and cylinder heads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on low and high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Al-249. Producer or source: Various aluminum companies.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (10): CS-213.
Published: 01 October 2021
... S.p.A., 2018, except where noted. Valid for steel grade C60E. Index of machinability is based on a value of 100% for SAE 1212 steel. Machinability Ratings for Cold-Drawn Steel Bars, Lucefin S.p.A. ISSN: 002-614X CS-213B ...
Abstract
View article
PDF
Lucefin C60, C60E, and C60R are high-carbon, non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. C60E and C60R may also be flame or induction hardened. C60, C60E, and C60R are used for applications where the higher carbon is needed to improve wear characteristics and where strength levels required are higher than those attainable with the lower carbon grades. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-213. Producer or source: Lucefin S.p.A.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (7): CS-227.
Published: 01 July 2022
... properties thermal properties UNS G10180 SAE 1018, CEN C17, ISO C17 STEEL DATA SURVEY (Wrought Low-Carbon Non-Alloy Steels) Filing Code: CS-227 Carbon Steel :: July 2022 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: matinfo@asminternational.org Published by ASM...
Abstract
View article
PDF
1018 and C17 are wrought low-carbon non-alloy steels that are used in the as rolled, normalized, or cold worked condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-medium strength, good cold formability, and excellent weldability are required. They may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-227. Producer or source: Data Survey.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (6): CS-224.
Published: 01 June 2022
... tensile properties thermal properties wear resistant alloys UNS G10100 SAE 1010, CEN C10, ISO C10 STEEL DATA SURVEY (Wrought Low-Carbon Non-Alloy Steels) Filing Code: CS-224 Carbon Steel :: June 2022 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: matinfo...
Abstract
View article
PDF
1010, C10E, and C10R are wrought low-carbon non-alloy steels that are used in the as rolled, annealed, normalized, or cold worked condition. These steels are widely used for lightly stressed parts that require excellent cold formability and excellent weldability. They are less expensive than 1008 / C8C and can be used when the requirements for cold forming are less exacting. C10, C10E, and C10R may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance and wear resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-224. Producer or source: Data Survey.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (6): CS-225.
Published: 01 June 2022
... properties thermal properties UNS G10150 SAE 1015, CEN C15, ISO C15 STEEL DATA SURVEY (Wrought Low-Carbon Non-Alloy Steels) Filing Code: CS-225 Carbon Steel :: June 2022 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: matinfo@asminternational.org 1015, C15E...
Abstract
View article
PDF
1015, C15E, and C15R are wrought low-carbon non-alloy steels that are used in the as rolled, annealed, normalized, or cold worked condition. These steels are widely used for lightly stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low strength, excellent cold formability, and excellent weldability are required. They may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-225. Producer or source: Data Survey.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (7): CS-226.
Published: 01 July 2022
... properties thermal properties UNS G10160 SAE 1016, CEN C16, ISO C16 STEEL DATA SURVEY (Wrought Low-Carbon Non-Alloy Steels) Filing Code: CS-226 Carbon Steel :: July 2022 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: matinfo@asminternational.org Published by ASM...
Abstract
View article
PDF
1016, C16E, and C16R are wrought low-carbon non-alloy steels that are used in the as rolled, normalized, or cold worked condition. These steels are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low strength, excellent cold formability, and excellent weldability are required. They may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-226. Producer or source: Data Survey.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (5): CS-223.
Published: 01 May 2022
... treatability joinability machinability physical properties tensile properties thermal properties UNS G10210 UNS G10220 SAE 1021, SAE 1022, CEN C20C, ISO C20C STEEL DATA SURVEY (Wrought Low-Carbon Non-Alloy Steels) Filing Code: CS-223 Carbon Steel :: May 2022 Materials Park, Ohio 44073-0002, USA...
Abstract
View article
PDF
1021, 1022, C20C, and C20GC are wrought low-carbon non-alloy steels that are used in the as rolled, normalized, cold worked, or quenched and tempered condition. They are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-moderate strength, good ductility, good cold formability, and good weldability are required. 1021 and 1022 may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-223. Producer or source: Data Survey.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2022) 71 (5): CS-222.
Published: 01 May 2022
... physical properties tensile properties thermal properties UNS G10200 SAE 1020, CEN C22 STEEL DATA SURVEY (Wrought Low-Carbon Non-Alloy Steels) Filing Code: CS-222 Carbon Steel :: May 2022 Materials Park, Ohio 44073-0002, USA :: +1.440.338.5151 :: www.asminternational.org :: matinfo...
Abstract
View article
PDF
1020, C22, C22E, and C22R are wrought low-carbon non-alloy steels that are used in the normalized, cold worked, or quenched and tempered condition. These steels are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-moderate strength, good toughness, good cold formability, and good weldability are required. They may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered condition for parts requiring a hard, wear-resistant surface, but where the core strength is not critical. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-222. Producer or source: Data Survey.