... 1074, C75S, and S75C are wrought high-carbon (carbon = 0.70–0.80%) non-alloy steels that are, in general, used in the cold worked, quenched and tempered, or austempered condition. These steels are widely used for highly stressed parts that require higher strength levels than can be achieved...