Skip Nav Destination
Close Modal
Search Results for
S22C
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
S22C
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (2022) 71 (11): CS-235.
Published: 01 November 2022
... 1023 and S22C are wrought low-carbon non-alloy steels (C = 0.20–0.25%, Mn = 0.30–0.60%) that are used in the as rolled, normalized, or cold worked condition. These steels are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower...
Abstract
View article
PDF
1023 and S22C are wrought low-carbon non-alloy steels (C = 0.20–0.25%, Mn = 0.30–0.60%) that are used in the as rolled, normalized, or cold worked condition. These steels are widely used for lightly and moderately stressed parts that require higher strength levels than can be achieved by the lower carbon grades, and also for applications where a combination of low-to-medium strength, good cold formability, and good weldability are required. They may also be used in the carburized or carbonitrided, and subsequently quench hardened and tempered, condition for parts requiring a hard, wear-resistant surface, but with little need for increased mechanical properties in the core. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CS-235. Producer or source: Data Survey.