Alloy Digest (2020) 69 (6): Al-465.
Published: 01 June 2020
... Rio Tinto 304.1 is a heat-treatable, aluminum-silicon casting alloy that also contains small amounts of iron, manganese, magnesium, copper, and titanium. This alloy is available in the form of ingots for remelting, for the manufacture of die castings. Alloy 304.0 was developed as K-Alloy by Delphi...