Alloy Digest (2022) 71 (5): Al-487.
Published: 01 May 2022
... Rheinfelden Anticorodal-04 (AlSi0.5Mg) is a heat-treatable aluminum-silicon-magnesium casting alloy that is used for applications requiring medium strength, excellent electrical conductivity, and excellent corrosion resistance. This alloy is, however, difficult to cast owing to its low silicon...