Alloy Digest (1966) 15 (7): Cu-166.
Published: 01 July 1966
... Revere No. 145 is a free-cutting grade of copper recommended for high conductivity parts, such as electrical connectors, relays, fasteners, contacts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...