Alloy Digest (1964) 13 (11): SA-170.
Published: 01 November 1964
... Republic HP150 is an alloy steel designed to give 150,000 psi yield strength with exceptional toughness. The alloy is intended for fabrication in the heat treated condition principally for heavy plate sections. This datasheet provides information on composition, physical properties, hardness...