Alloy Digest (1965) 14 (8): SA-181.
Published: 01 August 1965
... Republic HP 9-4-25 is a heat treated alloy steel capable of developing yield strengths up to 200,000 psi with toughness characteristics better than other quench and tempered alloys. It is designed for sheet, plate and forging applications. It is also designed to be welded in the heat treated...
Journal Articles
Alloy Digest (1972) 21 (7): SA-278.
Published: 01 July 1972
... REPUBLIC HP 9-4-30 is a heat-treated alloy steel capable of developing minimum yield strengths up to 190,000 psi with superior toughness characteristics. It is designed for sheet, plate, and forging applications, and can be welded in the heat-treated condition. The good thermal stability...
Journal Articles
Alloy Digest (1971) 20 (12): SA-270.
Published: 01 December 1971
... REPUBLIC HP 9-4-20 is designed especially for applications requiring optimum combinations of relatively high yield strength and toughness with good weldability. This alloy is capable of providing 180,000 psi yield strength in combination with a Charpy V-notch value of 50 ft-lb at 75 F in plate...