Alloy Digest (1967) 16 (1): SA-205.
Published: 01 January 1967
... Republic 50 is a high-strength low-alloy structural steel recommended where high yield strength and toughness combined with good weldability and corrosion resistance are required. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and...
Journal Articles
Alloy Digest (1971) 20 (12): SA-270.
Published: 01 December 1971
... REPUBLIC HP 9-4-20 is designed especially for applications requiring optimum combinations of relatively high yield strength and toughness with good weldability. This alloy is capable of providing 180,000 psi yield strength in combination with a Charpy V-notch value of 50 ft-lb at 75 F in plate...
Journal Articles
Alloy Digest (1972) 21 (10): SA-282.
Published: 01 October 1972
... Corporation. Producer or Source: Republic Steel Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity fracture toughness heat treatability joinability machinability Maxi-form 50 physical properties tensile...
Journal Articles
Alloy Digest (1974) 23 (8): SA-307.
Published: 01 August 1974
... FOR WELDING* Plate Thick- ness in. 318 112 314 1 Minimum Preheat and Interpass Temperature, oF Submerged-kc Process Shielded Metal Arc Gas Metal Arc Single Pass Mutiple Pass Single Multiple Single Multiple Neutral AUOY Neutral .-OY Pass Pass Pass Pass Flux Flux Flux Flux -- P--P 50 300 50 200 50 100...
Journal Articles
Alloy Digest (1964) 13 (11): Ti-42.
Published: 01 November 1964
... solutions. It is highly resistant co many acids, alkalis and ocher chemicals. It is slightly attacked by boiling 50% formic acid and heavily attacked by phosphoric acid. It resists oxidarion for prolonged exposures up co 8000F. It is completely resistant co sulphurous acid and is superior co stainless steel...
Journal Articles
Alloy Digest (1972) 21 (7): SA-278.
Published: 01 July 1972
...-16 Reduction of area, % 25-35 35-50 Charpy impact (V-notch) ft-lb 15-20 18-25 K Fa igue strength (107 cycles ), psi (No notch) 4 (Notch Bend), psi 600OCb90000 90000120000 - 120000 (Notched, Kt=3) - 55000 -f&la 3 - MINIMUM ROOM-TEMPERATURE MECHANlCAL PROPERTIES (Quenched to martensite and double...
Journal Articles
Alloy Digest (1965) 14 (7): SA-179.
Published: 01 July 1965
... 290000 250000 140000 260000 50 0.180 290000 250000 110000 170000 600 0.080 250000 235000 170000 250000 2; 0.180 250000 235000 165000 245000 65 Isothermal Treatment,oF (Bainite) 475 0.080 27 0000 225000 200000 270000 100 0.180 270000 225000 190000 245000 100 *Fatigue cracked center-notched specimens...
Journal Articles
Alloy Digest (1955) 4 (10): Ti-7.
Published: 01 October 1955
... :i s: ii 2 700 50 Table 3 - HEAT TREATED TENSILE PROPERTIES (Typical Data for Fine Grained Material) (14500P., 2 hours Water Quench and Draw) Yield SlXtlgtb psi 19sooo :;Eii 187000 175000 173000 164000 162000 160000 158000 4 24 4 24 4 24 4 24 4 24 204000 200000 198000 191000 181000 178000 168000...
Journal Articles
Alloy Digest (1960) 9 (5): SA-98.
Published: 01 May 1960
... particular y trans- portation units and materials handling equi ent. The high strength and toughness of this stee, combined p with a resistance to corrosion much higher than that of ordinary c savings in xe per-bearing steels, make possible weight for equipment. range of 40% to 50% and longer life Forms...
Journal Articles
Alloy Digest (1960) 9 (9): SA-104.
Published: 01 September 1960
..., particularly trans- portation units and materials handling equip ment. The high strength and toughness of this steel, combined with a resistance to corrosion much higher than that of ordinary copper-bearing steels, make possible weight savings in the range of 40% to 50% and longer life for equipment. Forms...
Journal Articles
Alloy Digest (1967) 16 (5): SA-209.
Published: 01 May 1967
...- chlorinated oils for rough turoiog; and use I50- 300 sfpm cutting speed, 0.0025-0.0035 ipr feed, 0.10-0.60 inch depth of cut with carbide (C-2) tools and heavy duty water soluble oils for finish turoiog. Drilling should be performed with cobalt type high-speed steel drills at 30-50 sfpm speed, 0.002-0.009 ipr...
Journal Articles
Alloy Digest (1969) 18 (8): SA-242.
Published: 01 August 1969
.... IS-20 Reduction of area, % 65-75 Rockwell hardness C28-30 Table 2 - TYPICAL MARAGED PROPERTIES (Annealed, then maraged at 9OOoF for 3 hours) Tensile strength, psi 265000-305000 Yield strength. psi (0.25,) 26000@300000 Elongation, % in 2 in. 3-10 Reduction of area, c*c 20-50 Notch T.S. to T.S. ratio...
Journal Articles
Alloy Digest (1960) 9 (1): Ti-23.
Published: 01 January 1960
... cuts 200400 sfpm Roughing cuts 100-150 sfpm Feed 0.010 to O.lO /rev. HighSpad FiiCUtS4040Sfirm Roughing cats 30-50 sfpm Feed 0.010 to O.lO /rev. sdfurhxd oil8 have beul used atensively as cuttiug fluids. C& cooIing has also proved successful for some applications. For e&c&e coolhg it is de&able that...
Journal Articles
Alloy Digest (1963) 12 (7): SA-149.
Published: 01 July 1963
...- al carbon steel, and approximately 50% greater than that of ASTM-All3 structural carbon steel. As indicated by Chatpy keyhole notched-bar impact tests, this steel has notch toughness or resistance to impact-type loading approximately 20% greater than that of structural carbon steel (ASTM-A;) at room...
Journal Articles
Alloy Digest (1962) 11 (10): SS-137.
Published: 01 October 1962
...-2650 Modulus of elasticity, psi I 106 30.5 Electrical resisciviry, microhms/in3 30.5 Magnetic permeability 1.001 PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES - Annealed Tensile strength, psi 90000-l 10000 Yield point, psi 40000-60000 Elongation, % in 2 45-55 Reduction of area, % 50-65 Brine11...
Journal Articles
Alloy Digest (1957) 6 (12): SS-65.
Published: 01 December 1957
... room temperature Elongation, 90 in 2 B56 sooE is 85 ft. lbs. minimum.) Rockwell hardness B90 % Cold Reduction 0 (annealed) 5 :: 30 50 Table 3-EFFECT OF COLD ROLLING-STRIP (Annealed material) (Single rest results) Tensile Yield Strength Strength psi psi (0.2%) 108170 51560 118050 81120 127100 94980...
Journal Articles
Alloy Digest (1968) 17 (4): SS-207.
Published: 01 April 1968
... TEMPERATURE PROPERTIES fAnnealed material) Test Tensile Temperature Strength OF psi 0 96000 -100 118000 -200 145000 -300 175000 -400 215000 Yield Screnath Elongation psi (O.Z%) % ii 2 45000 67 55000 65 68000 62 78000 59 89000 56 Annealed 80000-90000 35000-55000 70-50 7560 135-185 B70-90 120-70 Cold Rolled...
Journal Articles
Alloy Digest (1955) 4 (2): SS-25.
Published: 01 February 1955
... - TUBING AND WIRE PROPERTIES Tubing Wire Anneals Cold Drawn 65% 83000 135000 55000 115000 25 50 175 Table 3 - BAR AND ROD PROPERTIES Forged, Rolled and Annealed 75000-95000 45000-60000 25-35 45-65 160-200 0.050 0.058 0.0000058 0.0000063 29,000,000 Plate Annealed 85000 55000 25 B83 180 2 Wire Annealed 90000...
Journal Articles
Alloy Digest (1955) 4 (10): SS-35.
Published: 01 October 1955
... and coolant Approximate Cutting Speeds with HSS Tools Operatioo Speed, sfm Automatic screw machine Turret lathe :g::g Shaving or skiving 120-150 Milling 50-80 Drilling FgY:; g lo-25 2s;; lo-25 15-30 Cutting rates may be greatly increased with carbide tools, when applicable. Cast alloy or carhide tools...
Journal Articles
Alloy Digest (1961) 10 (6): SS-118.
Published: 01 June 1961
... 1000 1100 1200 1300 1400 Tensile strength, psi Annealed Cold Drawn 120000 130000 Yield point, psi 65000 115000 Elongation, % in 2 15-25 15 Reduction of area, % 60 58 Brine11 hardness 230 min. 270 Rockwell hardness C29 C40 min. lzod impact, ft. lbs. 50-80 Table 2 - SHORT-TIME ELEVATED TEMPERATURE...