Alloy Digest (1995) 44 (10): SS-615.
Published: 01 October 1995
... REMANIT 4003 possesses good workability, weldability and is mainly used in the transportation industry. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat...