Journal Articles
Alloy Digest (1954) 3 (4): Ti-3.
Published: 01 April 1954
... Rem-Cru C-130AM titanium-base alloy was developed with a minimum yield strength of 130,000 psi for fabrication into bars and forgings. It was formerly known as Rem-Cru RC-130B. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...