Alloy Digest (2000) 49 (6): SS-790.
Published: 01 June 2000
... RAM 316L is a machining-quality version of standard austenitic stainless steel type 316L. The alloy is designed to increase productivity and efficiency by allowing one to machine at higher speeds and feeds with less tool wear. This datasheet provides information on composition, physical properties...