Alloy Digest (2021) 70 (9): Al-480.
Published: 01 September 2021
... Raffmetal EN AB-Al Si7Mg0.3 (EN AB-42100) is a heat-treatable, Al-Si-Mg casting alloy in ingot form for remelting. It is used extensively for producing sand, permanent mold and investment castings for applications requiring a combination of excellent casting characteristics, high strength...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (12): Al-483.
Published: 01 December 2021
...; high strength strength higher than that of EN AC-Al Si7Mg0.3 (EN AC-42100); excellent ductility (shock resistance); good corrosion resistance; good machinability (after heat treatment); good weldability. See Table 3 for ratings of casting characteristics and other properties. Table 3 Casting...