Alloy Digest (2023) 72 (8): Al-501.
Published: 01 August 2023
... Raffmetal EN AB-Al Si10Mg(Fe) (EN AB-43400) is an aluminum-silicon-magnesium casting alloy in ingot form for remelting. It is used extensively for producing high pressure die castings and low pressure die castings for applications requiring a combination of excellent casting characteristics, good...